| Property | Value |
|---|---|
| Mechanical Properties | |
| Ultimate tensile strength | 758 – 860 MPa |
| Yield strength | 420 – 470 MPa |
| Young’s modulus (modulus of elasticity) | 190 GPa |
| Elongation at break | 16 % |
| Physical Properties | |
| Magnetism | Magnetic |
| Weldability | Poor |
| Thermal Properties | |
| Maximum service temperature | 195 – 245 °C |
| Thermal expansion coefficient | 10.3 – 12 × 10-6/ºC |
| Thermal conductivity | 29.3 – 31.7 W/(m⋅°C) |
| Electrical Properties | |
| Electrical resistivity | 65 – 70 μΩ*cm |
| Post Treatments | |
| Post-Processing | Hardening & Annealing |
| Anodizing compatibility | Not suitable |
| Common Applications | |
| Hot forging tools and dies | Hot extrusion tools and dies |
| Cold forming dies | |