| Property | Value |
|---|---|
| Mechanical Properties | |
| Ultimate tensile strength | 560 – 800 MPa |
| Yield strength | 340 – 430 MPa |
| Young’s modulus (modulus of elasticity) | 204 – 215 GPa |
| Elongation at break | 14 – 18 % |
| Physical Properties | |
| Corrosion resistance | Moderate |
| Magnetism | Magnetic |
| Weldability | Poor |
| Thermal Properties | |
| Thermal expansion coefficient | 10 – 10.2 × 10-6/ºC |
| Thermal conductivity | 22 – 24.2 W/(m⋅°C) |
| Electrical Properties | |
| Electrical resistivity | 60 μΩ*cm |
| Post Treatments | |
| Post-Processing | Cold and hot working, Annealing, Tempering, Hardening |
| Anodizing compatibility | Not suitable |
| Common Applications | |
| Gage blocks | Ball bearings and races |
| Molds and dies | Valve components |
| Measuring instruments | |