| Property | Value |
|---|---|
| Mechanical Properties | |
| Ultimate tensile strength | 900 – 930 MPa |
| Yield strength | 490 – 510 MPa |
| Young’s modulus (modulus of elasticity) | 190 – 200 GPa |
| Elongation at break | 40 – 45 % |
| Hardness | 40 HRC |
| Physical Properties | |
| Corrosion resistance | Excellent |
| Magnetism | Non-magnetic |
| Weldability | Excellent |
| Thermal Properties | |
| Thermal conductivity | 11 – 11.4 W/(m⋅°C) |
| Electrical Properties | |
| Electrical resistivity | 125 μΩ*cm |
| Post Treatments | |
| Post-Processing | Cold & hot working, annealing and aging |
| Anodizing compatibility | Not suitable |
| Common Applications | |
| Jet engines | Rocket motors |
| Spacecraft | Space shuttles |
| Nuclear reactors | Pumps & turbo pumps |
| Tooling | |