Property | Value |
---|---|
Mechanical Properties | |
Ultimate tensile strength | 520 – 560 MPa |
Yield strength | 460 – 470 MPa |
Elongation at break | 6 – 9 % |
Thermal Properties | |
Thermal conductivity | 130 W/(m⋅°C) |
Post Treatments | |
Anodizing compatibility | Not recommended – due to the high amount of zinc that the material contains, dark spots or corroded marks may be observed |
Common Applications | |
Fuse parts | Structural components |