Property | Value |
---|---|
Mechanical Properties | |
Ultimate tensile strength | 620 – 700 MPa |
Yield strength | 425 – 500 MPa |
Young’s modulus (modulus of elasticity) | 195 – 205 GPa |
Elongation at break | 14 – 28 % |
Physical Properties | |
Corrosion resistance | Excellent |
Magnetism | Magnetic |
UV resistance | Excellent |
Weldability | Good |
Thermal Properties | |
Maximum service temperature | 335 – 365 °C |
Thermal expansion coefficient | 13.5 – 18.2 × 10-6/ºC |
Thermal conductivity | 14.4 – 15.6 W/(m⋅°C) |
Electrical Properties | |
Electrical resistivity | 78.4 – 81.6 μΩ*cm |
Post Treatments | |
Post-Processing | Hardening |
Anodizing compatibility | Not suitable |
Common Applications | |
Environments containing chlorides and hydrogen sulphide | Flue gas filters |
Chemical tanks | Heat exchangers |
Acetic acid distillation components |