Property | Value |
---|---|
Mechanical Properties | |
Ultimate tensile strength | 790 – 1200 MPa |
Yield strength | 520 – 860 MPa |
Young’s modulus (modulus of elasticity) | 197 – 207 GPa |
Elongation at break | 3 – 16 % |
Physical Properties | |
Corrosion resistance | Excellent |
Magnetism | Magnetic |
UV resistance | Excellent |
Weldability | Moderate |
Thermal Properties | |
Maximum service temperature | 282 – 316 °C |
Thermal expansion coefficient | 12.5 – 13.1 × 10-6/ºC |
Thermal conductivity | 17.3 – 18.7 W/(m⋅°C) |
Electrical Properties | |
Electrical resistivity | 75 – 85 μΩ*cm |
Post Treatments | |
Post-Processing | Not suitable |
Anodizing compatibility | Not suitable |
Common Applications | |
Aerospace applications | Base plates |
Chemical processing equipment | Oil and petroleum refining equipment |