Property | Value |
---|---|
Mechanical Properties | |
Ultimate tensile strength | 330 – 350 MPa |
Yield strength | 140 – 150 MPa |
Elongation at break | 20 – 23 % |
Physical Properties | |
Corrosion resistance | Moderate |
Magnetism | Non-magnetic |
Weldability | High |
Post Treatments | |
Post-Processing | Annealing |