Property | Value |
---|---|
Mechanical Properties | |
Ultimate tensile strength | 520 – 560 MPa |
Yield strength | 460 – 470 MPa |
Young’s modulus (modulus of elasticity) | 69 – 76 GPa |
Elongation at break | 6 – 9 % |
Physical Properties | |
Corrosion resistance | Moderate |
Magnetism | Non-magnetic |
Weldability | Poor |
Thermal Properties | |
Maximum service temperature | 100 °C |
Thermal expansion coefficient | 22.9 – 24.1 × 10-6/ºC |
Thermal conductivity | 131 – 137 W/(m⋅°C) |
Electrical Properties | |
Electrical resistivity | 5.2 μΩ*cm |
Post Treatments | |
Post-Processing | Annealing & Cold working |
Anodizing compatibility | Not recommended – due to the high amount of zinc that the material contains, dark spots or corroded marks may be observed |
Common Applications | |
Aircraft and aerospace | Marine |
Transportation |