Property | Value |
---|---|
Mechanical Properties | |
Ultimate tensile strength | 355 – 370 MPa |
Yield strength | 230 MPa |
Young’s modulus (modulus of elasticity) | 190 – 210 GPa |
Elongation at break | 18 – 26 % |
Physical Properties | |
Corrosion resistance | Moderate |
Magnetism | Magnetic |
Weldability | Poor |
Thermal Properties | |
Thermal expansion coefficient | 11.5 – 13.9 × 10-6/ºC |
Thermal conductivity | 51.9 W/(m⋅°C) |
Electrical Properties | |
Electrical resistivity | 17.4 μΩ*cm |
Post Treatments | |
Post-Processing | Cold working |
Anodizing compatibility | Not suitable |
Common Applications | |
Marine engineering | Furnaces and gas turbines |
Chemical processing plants | Boiler and pressure vessels |
Nuclear power plants |